1 |
size(LxHxB) |
625mm * 240mm * 75mm-300mm |
255mm * 75mm * 105mm |
2 |
Precision in size |
variation 1.00(+/-) |
Variation 2.15 (+/-) |
3 |
Compressive Strength |
3-4.0N/mm2 (As per IS:2185 part III |
2.5-3.0 N/mm2 |
4 |
Dry Density |
550-650kg/m3(Oven dry) |
1800 kg/m3 |
5 |
Fire Resistance |
2 to 6 Hours depending on thickness |
2Hours |
6 |
Sound Reduction index 1(dB) |
45 for 200 mm thick wall |
50 for 230 mm thick wall |
7 |
Thermal Conductivity. (Kw-m/C) |
0.16 |
0.81 |
8 |
Mortar Consumption M3 with 1.6 |
0.5 bag of Cement |
1.35 bag of Cement |
9 |
Construction Time per mason |
30 Sqm. |
20 Sqm. |
10 |
Chemical Composition |
Fly ash used around 70% which reacts with binders (Lime & Cement) to form AAC |
Soil is sued which contains many inorganic Impurities like sulfates etc resulting in Efflorescence |
11 |
Finishing |
Can be directly cut or shaped/sculptured as required |
Not Possible |
12 |
Contribution to carpet area |
3-5% |
No Contribution |
13 |
Cost benefit Factor |
Saving up to 24% in structural cost due to reduction of dead load (subject to project design) |
No Cost Benefit |
14 |
Energy saving |
Up to 30% of Air conditioning Load reduction |
No Energy Saving |